Edit: Thanks to everyone for the help! Just an update.

Thanks to @nate3d and @IMALlama comments below I calibrated the e-steps that were very under and it improved a lot.

I left the filament on the dryer for 8 hours and tested again with a 20mm /s speed and 220 C print temp and it was better (picture below)

Just to answer you all saying it’s a clog or a hot end problem, it’s not, the whole hot end, includong nozzle, heat block and everything else, even the PTFE tube are all brand new and I checked before.

This is still the best I could achieve and It took 3 hours to print this benchy lol

‐-------- Hi everyone, I’m once again asking for your help lol Since I’ve tried to print with wood I totally wrecked my printer so I changed the hot end and am trying to set it all up again. Since my printer already came built and working I don’t have much experience with things like this so if you could help me I would be very thankful

What do I need to twerk to make it print better again?

I’m using Cura slicer and trying to print a benchy with the settings below:

Nozzle: 0.4

Layer: 0.2

Printing temp: 220 (it wont print with lower temp)

Speed: 60

Retraction distance: 7

Retraction speed: 70

Edit: PLA

  • atocci@lemmy.world
    link
    fedilink
    English
    arrow-up
    15
    ·
    edit-2
    4 months ago

    The fact it won’t print below 220° makes me think it’s a problem with your hotend, and my best guess is that your nozzle is clogged. The higher temperature might be helping the extruder to squeeze a bit of filament around the clog, but not enough.

    Changing the nozzle is quick and easy, and most printers come with a spare or two, so I would give that a shot before diving too deep into diagnostics.

    • froh42@lemmy.world
      link
      fedilink
      English
      arrow-up
      3
      ·
      edit-2
      4 months ago

      They might just try a cold pull or two before changing the nozzle. (Depening on the printer. On my Ender 3 Nozzle swaps were a no brainer - 2 minutes, on my current SV08 they are 15 min of work and 45 min of soaking the old nozzle in Isopropanol to get the thermistor out without ripping the cables)

      • atocci@lemmy.world
        link
        fedilink
        English
        arrow-up
        2
        ·
        4 months ago

        Wow I just looked it up and that is the worst design I’ve ever seen. That’s a ton of work just to replace one of the most commonly changed parts.